Home/Flooring Knowledge/Subfloor Flatness Guide
Artemis Flooring · Subfloor preparation guide

Your floor looks flat. Your slab probably isn't.

Hybrid flooring is rigid. It cannot follow humps and dips in the concrete underneath, so the slab has to be made flat first. This guide shows what we check, why it matters, and how we fix only what needs fixing.

We never pour compound over a floor we haven't investigated. Every Artemis proposal is based on what we measure on site, with the existing floor lifted.

1 · The illusion

Flat to the eye is not flat to a straightedge

A concrete slab is finished by hand. Standing in the room, a few millimetres of rise and fall across several metres is invisible, especially under carpet or old flooring.

Lay a long straightedge on the bare slab and the humps and dips show up straight away. The drawing exaggerates the height so you can see them.

What your eye sees What a straightedge finds (height exaggerated) hump dip hump dip
Same slab, two views. The dashed blue line is the flat plane a new floor needs.
2 m straightedge gap measured here concrete slab
The straightedge rests on the high points. The gap under it is the number that matters.
2 · The test

How flat is flat enough?

The Australian Standard for resilient flooring, AS 1884:2021, sets the baseline: no more than 4 mm of gap under a 2 m straightedge. For scale, 3 mm is about the thickness of a $1 coin.

Many hybrid manufacturers ask for tighter than the standard, and their written tolerance is what protects your warranty. We measure against the guide for the exact product you choose.

Published byMaximum gap
AS 1884:20214 mm under 2 m
Godfrey Hirst hybrid2 mm over 1 m
National Select hybrid3 mm over a 3 m diameter
3 · The consequence

What an uneven slab does to hybrid boards

A hybrid board has a stone-and-plastic core. It stays straight, so over a dip it bridges the gap and leaves a hollow underneath.

Every footstep then bends the boards at their click joints. Over time the joints loosen. You notice it as a hollow sound, a bouncy patch, boards that click, or seams that start to open.

Sources: Flooring Surgeons, Online Flooring Store

footstep click joint flexes hollow dip in the slab
The board bridges the dip. The joint above the hollow takes the load with nothing under it.
Example heat map, living room (mm from flat)
high spot (+) low spot (−) within tolerance
Illustration only, not a real job. It shows the idea: one hump near the top, one low corner on the right, and most of the room already fine.
4 · The Artemis approach

Lift, measure, map. Then propose.

You can't measure a slab through carpet. We lift the existing floor first. A straightedge only shows the strip it is resting on, so it can miss a hump or dip between passes. We set a self-levelling laser at the centre of the room and measure outwards from it, point by point. Those readings make the heat map of the slab.

Measuring from a laser is the Artemis method. The pass mark is still the gap under a straightedge, because that is how the standard and the product guides write it.

That map decides the treatment. Most rooms need work in a few places, not everywhere. A blanket pour over an unmeasured floor costs you compound you didn't need and can still leave a hump sitting under it.

One Australian testing lab reports a job where a 6 mm gap under the straightedge meant the finished floor had to be removed and the slab rectified. Source: ATTAR

5 · The treatments

Six fixes, matched to what we find

Grey is your slab. Orange is the problem. Blue is what we add. The standard's own remedy has two halves: high points are ground down and low points are filled.

Which fix for which depth
Feather finish
0 to 3 mm, local
Skim topping
up to 3 mm, across a room
Patch and ramp
2 mm and deeper, local
Full levelling pour
over 5 mm, widespread
0 mm3510 mm+
Depth bands are Artemis practice. The pass mark is always your product's written tolerance.

Grind the high spots

When: a hump or ridge sits above the rest of the slab.

Removing a hump is often better than burying it. Filling up to the height of a hump raises the whole floor and uses far more compound.

Houses on a ground slab. Apartments need approval first, see section 6.

Feather finish

When: a shallow dip that falls away in one direction.

A trowelled compound that tapers to nothing at its edges, so it blends into the slab with no step. Used only where the dip is.

Ardex rates Feather Finish from a feather edge up to 3 mm in one application. Datasheet

Patch and ramp

When: a deeper hollow in one spot, or a height step at a doorway.

A stiffer repair mortar that holds its shape in thicker fills. It fills the hollow or forms a gentle ramp between two levels.

Ardex lists its A 45 patching and ramping compound at 2 to 30 mm in one application. Product booklet

Skim topping, to 3 mm

When: many small ripples spread across a room, none of them deep.

One thin trowelled layer over the area takes out the ripples without the volume of a poured leveller. This is where most of the compound saving comes from.

Artemis method.

Full levelling pour

When: height differences over 5 mm that run through the property.

A self-levelling compound is poured across the floor and finds its own level. It is the right answer for a badly uneven slab, and the wrong first move for a floor with three dips.

The 5 mm trigger is Artemis practice, applied after measuring.

Moisture check and primer

When: every job, before any compound goes down.

A slab that is damp or dusty will let go of whatever is stuck to it. We test moisture to AS 1884 and prime as the compound's datasheet requires, so the fix stays bonded.

Moisture limits vary by product. We use the limit in your flooring's guide.

Flat is not the same as level

A slab can pass the flatness test and still fall steadily in one direction. The boards are fully supported, so the floor will perform. But you will see it: the finished floor runs uphill or downhill across the room.

If you want the floor to look as good as the money you are putting into it, a full levelling pour is the right fix. We still measure first, so the pour is only as deep as the slope needs and no compound is wasted.

Levelling a slab that already passes for flatness is your choice, not a product requirement. Recommending it is Artemis practice.

6 · House or apartment

The same hump, two different rules

In a house the ground slab is yours. In a NSW apartment the slab between units is common property, and it may contain steel cables under tension. That changes which fixes we can offer.

House, ground floor hump ground off your slab ground

Grind highs, fill lows

The slab sits on the ground and belongs to the owner. Grinding a hump is usually acceptable, and it keeps the finished floor height down at doorways.

Apartment your unit steel cables inside the slab neighbour's unit below common property

Fill by default, grind only with approval

New hard flooring in a NSW strata building needs owners corporation approval in any case. Grinding the slab alters common property, so it also needs strata approval and may need a structural engineer's sign-off, as your owners corporation sets.

Worth knowing: one strata lawyer's published view is that the owners corporation pays to re-level a slab that isn't fit for flooring. Our site report gives you the evidence to raise it.

General information, not legal advice. Check with your strata manager for your building. Sources: NSW Government, LookUpStrata, Jamesons Strata, Adams Stirling on post-tensioned slabs

7 · Laminate

Laminate: similar rules, a little more give

Laminate is also a floating click floor, so the same checks and the same six fixes apply. Its core is high-density fibreboard, a wood-fibre board, where hybrid has a stone-and-plastic core.

In our experience laminate boards flex slightly more and are less punishing over a minor dip. That is our observation on site. It never overrides the manufacturer's instructions, and published laminate tolerances are just as strict.

Example: Oakleaf laminate specifies no more than 3 mm over a 3 m radius. Install guide

Hybrid: stays straight, bridges the dip
Laminate: gives slightly, still unsupported
Either way the joint over the dip has nothing under it. The fix is the same: flatten the slab.
8 · Engineered timber

Engineered timber: real timber needs a flat slab too

Engineered timber is affected the same way. Most engineered boards join with a tongue and groove, not a click lock. When the floor is floated, the joints are commonly glued with PVA.

Over a dip the boards bridge the hollow, and every footstep works the glued joints. In our experience the glue line can crack, and the floor can start to creak or move.

Engineered timber is usually the most expensive of these floors. It is not the one to risk on a slab nobody has measured.

9 · Vinyl

Vinyl is a different world: flat is not enough, it must be smooth

Glue-down vinyl planks and sheet vinyl are thin and flexible. They don't bridge anything. They follow the subfloor exactly, so a ridge, a grout line or a trowel mark underneath becomes a visible line on top. The trade calls it telegraphing.

Telegraphing ridge shows grout line shows subfloor
The orange line is the vinyl. Whatever shape the subfloor has, the vinyl takes.
Two tests, not one 2 m straightedge: flat within 4 mm 150 mm straightedge: smooth within 0.5 mm
A slab can pass the long test and still fail the short one. Vinyl needs both.

The standard measures smoothness

AS 1884:2021 sets two limits for vinyl: flat within 4 mm over 2 m, and no abrupt deviation greater than 0.5 mm under a 150 mm straightedge. Half a millimetre is about five sheets of paper.

Source: Gibbon Architectural

Most complaints start here

An Australian flooring testing lab says most of the complaints it investigates come down to moisture, subfloor preparation, or a subfloor that wasn't smooth and flat.

Source: ATTAR

How vinyl preparation differs

Concrete or sheet flooring: skim the whole floor

With hybrid we treat the problem spots. With vinyl the entire surface has to be smooth, so a full skim coat is common.

The full skim coat is Artemis practice.

Over tiles: flood the grout lines

Grout lines show through vinyl, so tiles get a full coat of compound. Gerflor says to fill and smooth grout lines and textured surfaces.

Gerflor

Timber floors: sheet underlay first

Board edges and gaps would print through. Gerflor requires timber floors to be overlaid with hardboard or fibre cement underlay.

Gerflor

Sources

Standards and manufacturer documents are quoted for their published figures. Where a point is Artemis practice or experience, the page says so. Your product's installation guide always takes priority.

  1. AS 1884:2021 Floor coverings, resilient sheet and tiles, installation practices (Standards Australia)
  2. Subfloor preparation to AS 1884:2021 (Gibbon Architectural)
  3. Subfloor planeness and smoothness (ATTAR testing laboratory)
  4. Hybrid floors installation instructions (Godfrey Hirst)
  5. National Select Floors hybrid installation guide
  6. ARDEX Feather Finish datasheet
  7. ARDEX flooring products booklet
  8. Strata renovation rules (NSW Government)
  9. Who pays to re-level the slab (LookUpStrata)
  10. Sheet vinyl installation guide (Gerflor)